Omfattning
This European Standard defines the grades of abrasion resistant white cast irons. It specifies the grades in terms of: - chemical composition; - hardness. The types of abrasion resistant white cast irons covered by this standard are: a) unalloyed or low alloy cast irons; b) nickel-chromium cast irons covering two general types: - 4 % Ni 2 % Cr cast irons; - 9 % Cr 5 % Ni cast irons; c) high chromium cast irons covering four ranges of chromium content: - 11 % <- Cr =14 %; - 14 % <- Cr =18 %; - 18 % <- Cr =23 %; - 23 % <- Cr =28 %; and for each chromium content range, three ranges of carbon content.

Ämnesområden

Gjut- och tackjärn (77.080.10)


Köp denna standard

Standard Svensk standard · SS-EN 12513

Gjutning - Vitjärn
Prenumerera på standarden - Läs mer Dölj
Pris: 875 SEK
standard ikon pdf

PDF

Pris: 875 SEK
standard ikon

Papper

Fler alternativ Färre alternativ

Produktinformation

Språk: Engelska

Framtagen av: Gjutet järn och stål, SIS/TK 130

Internationell titel: Founding - Abrasion resistant cast irons

Artikelnummer: STD-30059

Utgåva: 1

Fastställd: 2001-04-12

Antal sidor: 14

Ersätter: SIS 140457 , SIS 140466 , SIS 140512 , SIS 140513

Ersätts av: SS-EN 12513:2011